HU Ji-xuan, ZHANG Qi, DENG Yin, ZHANG Lu-geng, HU Zhi, LIU Wei-cheng, ZHENG Dong-ming, TANG Xin-wen. Experimental Study of 30CrMnSiNi2A with Fatigue Damage Based on Two-dimensional Magnetic Memory Testing[J]. Failure Analysis and Prevention, 2014, 9(4): 218-223. DOI: 10.3969/j.issn.1673-6214.2014.04.006
    Citation: HU Ji-xuan, ZHANG Qi, DENG Yin, ZHANG Lu-geng, HU Zhi, LIU Wei-cheng, ZHENG Dong-ming, TANG Xin-wen. Experimental Study of 30CrMnSiNi2A with Fatigue Damage Based on Two-dimensional Magnetic Memory Testing[J]. Failure Analysis and Prevention, 2014, 9(4): 218-223. DOI: 10.3969/j.issn.1673-6214.2014.04.006

    Experimental Study of 30CrMnSiNi2A with Fatigue Damage Based on Two-dimensional Magnetic Memory Testing

    • The experiment selects different thickness of the 30CrMnSiNi2A flat notched specimens,which experiment with low cycle fatigue testing under the stress of 0. 7σs level, and conducts a two-dimensional magnetic memory testing, researchs the variation of magnetic memory signal under different cycles and different thickness. The experimental results show that: with the increase of the number of cycles, the characteristics of the magnetic memory signal of local stress concentration become more and more obvious, and the signal amplitude is also growing, the most significant characteristic phenomenon appears before the unstable crack fracture, which the normal component exists zero point, while the tangent component has max. The Logistic curve of the equivalent area of the closed field of the Lissajous synthesized by the differential of the normal and tangent component with cycles was fitting, it can be used to quantitative analysis the degree of fatigue damage. These results will provide technical support for further research on 2D testing of magnetic memory.
    • loading

    Catalog

      /

      DownLoad:  Full-Size Img  PowerPoint
      Return
      Return