彭云强,陈志,李建国,等. 螺栓连接结构轴向加载的疲劳失效[J]. 失效分析与预防,2025,20(4):317-324. doi: 10.3969/j.issn.1673-6214.2025.04.008
    引用本文: 彭云强,陈志,李建国,等. 螺栓连接结构轴向加载的疲劳失效[J]. 失效分析与预防,2025,20(4):317-324. doi: 10.3969/j.issn.1673-6214.2025.04.008
    PENG Yunqiang,CHEN Zhi,LI Jianguo,et al. Fatigue failure of bolt-connected structures under axial loading[J]. Failure analysis and prevention,2025,20(4):317-324. doi: 10.3969/j.issn.1673-6214.2025.04.008
    Citation: PENG Yunqiang,CHEN Zhi,LI Jianguo,et al. Fatigue failure of bolt-connected structures under axial loading[J]. Failure analysis and prevention,2025,20(4):317-324. doi: 10.3969/j.issn.1673-6214.2025.04.008

    螺栓连接结构轴向加载的疲劳失效

    Fatigue Failure of Bolt-connected Structures Under Axial Loading

    • 摘要: 螺栓连接是工业装备中应用最广泛的紧固连接方式之一,螺栓连接结构的疲劳可靠性对于服役装备的安全性至关重要。本文采用宏观试验和微观分析相结合的方法,对8.8级、12.9级螺栓和10.9级双头螺柱开展紧固件轴向疲劳性能测试,对同种材料经切削和滚压工艺加工的螺栓进行疲劳性能对比测试;另外,对螺栓连接模拟结构进行轴向疲劳性能测试,并借助超声预紧力监测设备确定螺栓的预紧力变化情况。结果表明:8.8级螺栓抗疲劳性能明显优于10.9级、12.9级高强螺栓,且在相同疲劳载荷幅条件下,8.8级螺栓疲劳寿命超过12.9级螺栓10倍有余;8.8级螺栓螺纹采用的滚压工艺制备,而10.9级和12.9级螺栓螺纹均采用切削工艺加工。对于同种材料的螺栓,采用滚压工艺加工的螺栓可以提升疲劳寿命5~10倍。在相同疲劳载荷水平下,紧固件疲劳寿命超过模拟连接结构7倍。

       

      Abstract: Bolted connection is one of the most widely employed fastening connections in industrial equipment. The fatigue reliability of bolted connection is critical to the operational safety of service equipment. This study integrates macroscopic experimentation with microscopic analysis to investigate the axial fatigue performance conducted on Class 8.8, Class 12.9 bolts, and Class 10.9 stud bolts. Comparative fatigue tests were conducted on bolts made of the same material but processed via cutting and rolling techniques. Additionally, axial fatigue tests were carried out on simulated bolted joint structures, and ultrasonic preload monitoring equipment was utilized to track changes in bolt preload. Experimental results indicate that the fatigue performance of Class 8.8 bolt is obviously better than that of Class 10.9 and 12.9 high-strength bolts. The fatigue failure life of Class 8.8 bolt is more than 10 times that of Class 12.9 bolt when they are subjected to the same fatigue load amplitude. The thread of Class 8.8 bolt is machined by the rolling process, while the threads of Class 10.9 and 12.9 bolts are machined by the cutting process. The test results of bolts made from the same material but processed by different methods reveal that the fatigue life of bolts machined by rolling process can be prolonged by 5~10 times. Under the same fatigue load level, the fatigue life of the fastener is over 7 times longer than that of the simulated connection structure.

       

    /